IBUMBA LYA MER: Ukwambilapo kwa Mupiipi ukwa Cishinte ca Kupanga Amapepala
Mu fikuulwa fya fimuti ifya nomba line, amabwe ya pellet yabomba nge cipimo ca pa muulu-umutolo wa cimuti icakubomfya ku kupanga icuma icakubomfya. Umulimo wa kupanga amapepala ya cimuti ulepanga umuunga uwasuma uwa cimuti mu maka ayakulisha, amapepala ayasuma aya muputule, ukupwisha ubwafya bwa kuti umuunga uwasuma te kuti ubikwe mu citofu. Ifunde lya iko ilya kubomba lyalipaatukana sana mu fiputulwa fine ifyacindama: ukupanga amabumba, ukuuma no kupya, ukufuuta ukwakulisha-, no kufuuta mu fipe fyapwa, ukupanga inshila iyakumanina iya kwalula umubili ne fya kemikali.
I. Inshita ya Kubemba: Ukupanga Amabola ya Katapa-katapa
The balling stage marks the beginning of the pelletization process. The core involves mixing fine iron concentrate powder (with particle size < 0.074mm accounting for >80%), ifibikilo (nga bentonite) na menshi mu cipe nangu mu cipe ca ng'oma, umo amabumba ya katapa-katapa ayashinguluka yapangwa ukupitila mu kupilibula kwa makanika na maka ya mishipa. Mu cituntulu, mwi samba lya mulimo wa maka ya kupilibula na ya ku nse, ifiputulwa ifituntulu filakonkana no kukula umuputule ne muputule ne ciputulwa icisuma nga pakati, ukupanga amabumba ya katapa-katapa ayakwata ubutali bwa 8-16mm. Mu fya kemikali, ifibumba ne menshi filapanga ifibumba fya menshi pa kati ka fipimfya, ukukosha amaka ya kubalilapo aya mabola ya katapakatapa ku kufikilisha ififwaikwa ifya kutwala ifyakonkapo no kupanga umulilo.
II. Iciputulwa ca Kuuma no Kufuuta: Ukufumya amenshi mu Mubili no Kukosha
Amabumba ya katapa-katapa yaingila mu cipe, apo amenshi ayabula ukulipila yafumishiwa mu ciputulwa ca kuuma pa madigiri 200-400 ku kucingilila ukuputuka pa kukaba ukwakulisha, elyo ukulonganika kwa kubalilapo kulapwishiwa mu ciputulwa ca kupya pa madigiri 900-1000 . Mu nshita iyi, amabwe ya magnetite (Fe3O4) mu mabola ya katapa-katapa yasansalikwa ku hematite (Fe2O3), kabili icakubikako cilapita mu fyakucita ifya kupanga amabumba ya kristalo aya kubalilapo, ukuwamya nga nshi amaka ya mabola ya katapa-katapa no kubika umufula wa kukoca ukwakonkapo.
III. Iciputulwa ca Kufuuta Icakulisha-Ukufuuta: Ukupanga Cipya Cipya Amakristalo no Kuwamya Amaka
Amabumba ya katapa-katapa ayafuuta kale yaingila mu citofu ica kupilibula nangu mu citofu ca kufimbapo pa kufimbapo pa madigiri 1200-1300, icintu icikalamba ica kupanga imibele ya mabwe ya pellet. Ifiputulwa fya hematite filabweluluka no kukula, ukupanga umusango wa kristalo uwafina; ifiko nga SiO2 na CaO mu ciputulwa ca nshita cipanga umutengo uunono uwa menshi, ayo ayasusha ifiputulwa fya fipimfya no kupanga umubili uwakosa uwakosa pa numa ya kutonta, ukushininkisha amaka ya kutonta no kucingililwa kwa mucinshi ukwa pellet ore. Pa nshita imo ine, cishininkisha ukuti amafuta ya cimuti yaonaika, ukuwamya umusango no kucefyako amabwe ya pellet.
IV. Iciputulwa ca Kutonsha: Ukuwamya kwa Mibombele
Iciputulwa ca mabwe icakosa icakosa (mupepi na madigili 1000-1100) cilaingila mu cipe cakutonsha, umo umwela uwatonta ulepuupuutulwa pakuti ucitontele ukufika ku madigiri 100-150. Ukufuuta bwangu bwangu kulacilikila ukukosa kwa kristalo, ukusunga umusango wa fimuti ifyafina no kukosa kwa pellet ore no kucingililwa ku konaula kwa fibombelo fyakonkapo. Umulilo uwaonaika uwakulisha pa madigiri 300-400 uwapangwa mu nshita ya kutonta kuti wabweshiwa ku cipe cakuumishishamo no kupyanika amabumba ya katapa-katapa, ukumfwikisha ukupita kwa maka no kucefyako ukubomfya kwa maka.
Ukupitila mu kucenjela bwino bwino ukutenta, umupashi ne nshita ya cila ciputulwa, inshila ya kupangamo ifipe ilapilibula umuunga uwacepa uwa cimuti icalinga ukuba ica mutengo uwa pa muulu. Ukulingana no bukulu bwa fipimfya no kucefyako bwino, kuti kwalenga ukusungusha kwa muputule wa mulilo ukuwama no busuma bwa cimuti icasunguluka, ukucilenga ukuba icacindama mu fyakupangapanga ifya muno nshiku ifya cimuti ne fimuti.